技術指標:
1:顆粒直徑:1.0-1.2mm 2:堆 比 重:620—650Kg/M3
3:吸附周期:1*50S 4:抗壓強度:35-80N/顆
5:抗壓磨耗:< 1 % 6: 含水率:< 0.5 %
型 號 | 吸附壓力Mpa | 氮濃度% | 產氮量M3/h.t | 空氮比% |
CMS-220 | 0.6 | 99.999 | 40 | 7.9 |
99.99 | 75 | 5.8 | ||
99.9 | 130 | 4.1 | ||
99.5 | 185 | 3.1 | ||
99.0 | 220 | 2.5 | ||
98.0 | 240 | 2.2 | ||
CMS-220 | 0.8 | 99.999 | 48 | 7.9 |
99.99 | 90 | 5.8 | ||
99.9 | 155 | 4.1 | ||
99.5 | 220 | 3.1 | ||
99 | 260 | 2.5 |